SPECIFICATION OF OXIDIZED BITUMEN 85/40
SPECIFICATION
TEST METHOD
Specific gravity@25/25 ˚C
1.05 approx
D-70
Penetration@25 ˚C
10-25
D-5
Softening point ˚C
85-95
D-36
Ductility@25 ˚C
3
D-113
Loss on heating (wt)%
0.5
D-6
Flash point ˚C
260 min
D-92
Solubility in CS2 (wt)%
99 min
D-4
OXIDIZED BITUMEN USAGE
Foundation damp-proofing
Built-up roofing systems.
Roll and pour application of bitumen felts.
Bonding of SBS modified membranes by hot mop method.
Sealing of laps and joints of various bituminous felts and membranes.
Wet area waterproofing.
Bonding of wooden boards insulation panels.
Road resurfacing and repair.